2507 Stainless Steel Coil Composition Content
Grade |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
N |
2507 |
Min. Max. |
≤0.03 |
≤1.2 |
≤0.80 |
≤0.035 |
≤0.02 |
24-26 |
3-5 |
6-8 |
0.24-0.32 |
SAF 2507 offers high compressive strength, impact strength, low coefficient of thermal expansion and high thermal conductivity.
These characteristics are applicable to many structural and mechanical components.
SAF 2507 has high impact strength and is not suitable for prolonged exposure to temperatures higher than 570°F, which may reduce toughness.
Tensile strength: σb≥ 730MPa;
Elongation: δ≥20%